Grind the Gum Rosin into powder, heat it up to be melted and then stir it, when the temperature up to 150-160°C, mix the melted rosin with maleic anhydride, and then heat it up to 190-200°C for chemical reaction for 1 hour.
Drop the phenolic condensation compound it to the melted gum rosin and heat them up to 230-240°C, add pentaerythritol and magnesium oxide into it for further reaction for 1 hour, and then raise it's temperature up to 270-280°C. Make it vacuumized when the acid number low down to 25mgKOH/g, keep the reaction going under the decompression until the acid number come to the desired value, the final process PhenolicResin Water Based Emulsion complete.